PA6/CM1011G-30/日本东丽
①原料描述部分
|
|||
规格级别
|
注塑 其它 其它
|
外观颜色
|
|
该料用途
|
|||
备注说明
|
特性:玻璃30%强化,高流动。
|
②加工条件
|
加工条件
|
性能项目
|
试验条件[状态]
|
测试方法
|
测试数据
|
数据单位
|
||||
基本性能
|
吸水率
|
23℃,24小时
|
|
%
|
||||
物理性能
|
比重
|
ASTM D-792
|
|
|||||
机械性能
|
IZOD冲击强度
|
无缺口1/8,23℃
|
|
kg·cm/cm2
|
||||
挠曲强度
|
80℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
抗剪强度
|
23℃
|
ASTM D-732
|
|
Kg/cm2
|
||||
断裂伸长率
|
80℃
|
ASTM D-638
|
|
%
|
||||
断裂伸长率
|
23℃
|
ASTM D-638
|
|
%
|
||||
洛氏硬度
|
23℃
|
ASTM D-785
|
|
R-标度
|
||||
洛氏硬度
|
23℃
|
ASTM D-785
|
|
M-标度
|
||||
抗拉屈服强度
|
80℃
|
ASTM D-638
|
|
Kg/cm2
|
||||
挠曲模量
|
-40℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
挠曲强度
|
23℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
压缩强度
|
-40℃
|
ASTM D-695
|
|
Kg/cm2
|
||||
压缩强度
|
80℃
|
ASTM D-695
|
|
Kg/cm2
|
||||
挠曲模量
|
80℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
断裂伸长率
|
-40℃
|
ASTM D-638
|
|
%
|
||||
挠曲模量
|
23℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
挠曲强度
|
-40℃
|
ASTM D-790
|
|
Kg/cm2
|
||||
抗剪强度
|
80℃
|
ASTM D-792
|
|
Kg/cm2
|
||||
压缩强度
|
23℃
|
ASTM D-695
|
|
Kg/cm2
|
||||
抗拉屈服强度
|
-40℃
|
ASTM D-638
|
|
Kg/cm2
|
||||
IZOD冲击强度
|
V-缺口1/2,-40℃
|
ASTM D-256
|
|
kg·cm/cm2
|
||||
泰伯磨耗量
|
(1000g,CS-17)23℃
|
ASTM D-1044
|
|
mg/1000次
|
||||
IZOD冲击强度
|
无缺口1/8,-40℃
|
|
kg·cm/cm2
|
|||||
IZOD冲击强度
|
V-缺口1/2,23℃
|
ASTM D-256
|
|
kg·cm/cm2
|
||||
抗拉屈服强度
|
23℃
|
ASTM D-638
|
|
Kg/cm2
|
||||
电气性能
|
抗电弧性
|
1/8"
|
ASTM D-495
|
|
秒
|
|||
介电常数
|
50Hz
|
ASTM D-150
|
|
|||||
体积电阻率
|
ASTM D-257
|
|
Ω.cm
|
|||||
损耗因数
|
50Hz
|
ASTM D-150
|
|
|||||
损耗因数
|
103Hz
|
ASTM D-150
|
|
|||||
介电常数
|
103Hz
|
ASTM D-150
|
|
|||||
损耗因数
|
106Hz
|
ASTM D-150
|
|
|||||
介电强度
|
1/8"
|
ASTM D-149
|
|
KV/mm
|
||||
介电常数
|
106Hz
|
ASTM D-150
|
|
|||||
热性能
|
导热系数
|
|
Kcal/m·hr·℃
|
|||||
熔点
|
差示扫描测热计DSC
|
|
℃
|
|||||
线性热膨胀系数
|
ASTM D-696
|
|
×10-5cm/cm/℃
|
|||||
热挠曲温度
|
4.6kg/cm2
|
ASTM D-648
|
|
℃
|
||||
UL-94抗燃级
|
UL 94
|
|
||||||
热挠曲温度
|
18.6kg/cm2
|
ASTM D-648
|
|
℃
|
||||
比热
|
|
Cal/g·℃
|
||||||
其它性能
|
强化含量
|
|
WT%
|