Tech-Rod 347 |
E347-16 |
0.55 |
1.65 |
0.52 |
19.15 |
10.15 |
|
铌稳定化不锈钢焊接321(18/8Ti),347,耐腐蚀性好,也可焊310,302,304,304L,308 |
Tech-Rod 385 |
E385-16 |
0.015 |
2.1 |
0.45 |
20.5 |
25.2 |
4.6 |
焊904L类不锈钢,制造储存硫酸磷酸容器设备等,抗应力腐蚀裂纹,耐点蚀隙蚀 |
Tech-Rod 410 |
E410-16 |
0.12 |
0.68 |
0.52 |
12.1 |
|
|
焊接403,405,410,416不锈钢,堆焊于碳钢上做耐腐蚀耐磨层,耐气蚀,耐淡水和弱酸侵蚀 |
Tech-Rod 410NiMo |
E410NiMo-16 |
0.03 |
0.52 |
0.45 |
12.1 |
4.55 |
0.52 |
焊接和补焊同材铸件,超低碳,抗裂性纫性均优于410,水轮机部件制造和维修的理想材料 |